| Customization: | Available |
|---|---|
| Type: | E (Carbon Steel Electrodes/ Low Alloy Steel Electrodes) |
| Material: | Steel Alloy |
| Shipping Cost: | Contact the supplier about freight and estimated delivery time. |
|---|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency





| Carbon steel welding electrodes | ||||||||
| Item NO. | GB/TB | AWS | ||||||
| J421 | E4313 | E6013 | ||||||
| Description: Pearlitic heat-resisting steel with coating of low sodium hydrogen electrode. DC reverse connection and all position welding. Workpiece shall be preheated about 150-250°C before welding and tempering at 620 710°C after welding process. |
||||||||
| Application: WER107 Heat-resistant Steel Electrode apply to weld the covering of the boiler pipes (e.g.15Mo) after argon arc render with working temperature below 510°C. Can also apply to weld general high strength low alloy steel. |
||||||||
| Chemical composition of Deposited metal(%): | ||||||||
| C | Mn | Si | Mo | P | S--- | |||
| ≤0.12 | ≤0.90 | ≤0.60 | 0.40-0.65 | ≤0.035 | ≤0.035 | |||
| Mechanical Performance of deposited Metal(690±15°C×1H tempering) | ||||||||
| Rm(Mpa) | ReL(Mpa) | A(%) | Akw(J) | |||||
| ≥490 | ≥390 | ≥22 | normal temperature | |||||
| ≥27 | ||||||||
| Deposited metal diffusion hydrogen content:≤6.0ml/100g (Method of glycerol) X ray flaw detection requirement:LevelI |
||||||||
| Reference Current:(DC) | ||||||||
| Diameter (mm) | Φ3.2 | Φ4.0 | Φ5.0 | |||||
| Current (A) | 90-120 | 140-180 | 170-210 | |||||
| Notes: (I)Please bake WER107 Heat-resistant Steel Electrode for 1 hour at about 350°C before welding. (II)Clean the surface to be welded thoroughly to remove surface contaminations |
||||||||